Boiler Plates

High-Temperature Certified Plates for Steam Generation & Heat Recovery

Boiler plates are specifically qualified for the fabrication of fired and unfired steam drums, boilers, and high-temperature pressure equipment. They are certified for elevated temperature tensile properties and are often subject to additional testing beyond standard PVQ plates.


Available Standards & Grades

Standard Grades Key Application
ASTM A515 Grade 60, 65, 70 Boiler drums and shells (intermediate to high temperature)
ASTM A516 Grade 60, 65, 70 Boilers requiring moderate/low-temperature notch toughness
ASTM A204 Grade A, B, C (C-0.5Mo) Elevated temperature boilers, waste heat recovery
ASTM A299 Grade A, B (Mn-Si) High-temperature boilers and pressure vessels
ASTM A302 Grade A, B, C, D (Mn-Mo, Mn-Mo-Ni) High-strength boiler applications
EN 10028-2 P235GH, P265GH, P295GH, P355GH European standard boiler and pressure vessel plates


Key Properties & Certifications

Requirement Detail
Elevated Temperature Tensile Certified yield and tensile properties at design temperature (typically up to 600°C)
Creep Resistance Long-term creep data available for chrome-moly and C-Mo grades
Notch Toughness Charpy V-Notch testing per specification (optional for standard grades)
Weldability Carbon Equivalent (CEV) typically ≤ 0.43-0.50 depending on grade
PWHT Simulated post-weld heat treatment testing available


Typical Applications in Oil & Gas

· Steam boiler drums (utility and package boilers)
· Waste heat recovery steam generators (HRSGs) in cogeneration
· Fired heater shells and tubesheets in refineries
· Steam injection boilers for thermal EOR (Enhanced Oil Recovery)
· Deaerator vessels
· Blowdown drums and flash tanks


Boiler Plate Grades Quick Reference

Grade Maximum Service Temp (approx.) Notes
A515 Grade 70 Up to 480°C The standard boiler plate
A204 Grade B (C-0.5Mo) Up to 520°C Improved creep resistance
A299 Grade A/B Up to 540°C Higher strength at temperature
A302 Grade B/C Up to 350°C High strength, lower temp